That’s right AS970 is now available through G&S Metals! The 97% silver casting grain is being sold as “Argentium Silver Casting Grain(tm)”. The following link will take you directly to the page that will tell you all about this wonderful new alloy. http://www.gsgold.com/castinggrain/argentium-silver.htm
If you love the look of fine silver, I think your going to love the look and durability of AS970.
At the time I checked the price of the casting grain it was the same price as fine silver casing grain.