June 20, 2005
From the picture above you can see I had a little trouble today. I was annealing a piece of Argentium to prepare it for hammering. I was working in fairly strong light and thought the piece had cooled sufficiently to allow me to quench it in water….Wrong! As you can see, the results were disastrous. [...]
Read the full article →
June 15, 2005
Last week I received my first shipment of Argentium Sterling® silver sheet and wire from Max And Me Beads. I only ordered a small amount (1.87 feet 10G round wire, 48 feet 24 G round wire, (1)6”x3” 30 G sheet, and (1) 6”x3” 24 G sheet). On the weekend I started on my new project. [...]