    Rex:In my experience,  Hide Glue works very well  for granulation. 
    Use about 2 drops of Hide Glue to 10 drops of water and about 3 drops
    of liquid (use an eye dropper).  I have used it on all my granulation
    and it never seemed noxious to me.  After applying the granules with
    the Hide Glue, place the whole piece on a small piece of ceramic tile
    and place near or under the small kiln or even an electric light
    bulb, so that it will dry off gradually. It is easiest to do this
    with a small (beehive kiln).  Once it is reasonably dry, place the
    ceramic piece with the granulated piece on it on top of the metal cap
    of the kiln.  When the Hide Glue is really dry it turns brown.  Once
    it has turned brown, remove it from the ceramic tile and place it in
    the kiln and put the cover on for a few seconds.  The Hide Glue will
    burn off, sometimes with brownish smoke, but very briefly.The trick
    in preventing the granules from popping off is to heat the whole
    piece very gradually.  Then, take the cover off, and the hide glue
    will have disappeared, and the granules are no longer glued to the
    backsheet.  Then heat with a large, bushy flame in a circular motion,
    etc., until the granules are fused.  Hope this helps  Sandra

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project