    having been to Doc's shop I can attest to his Laissez Faire (from
    the French, meaning to leave alone or to allow to do) attitude and
    use of chemicals which he has a grasp of in his rather laissez -faire
    way (from New Orleans Creole, meaning not to care -at all..or to
    trivialize) - it's not just theoretical chat folks- he cyanide bombs,
    he has mercury rolling around in a container, he has lots of things I
    inquired about the safety of (like the cyanide bombing pot without a
    lid next to the tanks of gas, and containers -open of course-in a bin
    that looked - dangerous at least, and hazardous at best with chemical
    crusts and salts all around everything that held or holds something!
    in way to small a space and with way to little air circulation in my
    opinion)..But the bottom line is He's still alive..Isn't it up to him
    how he chooses to perform his bench tasks..which from the evidence I
    saw he does very adeptly and customers keep coming back...that says a
    lot in itself..no one of them has (yet) died from having their ring
    bombed nor entering or exiting his shop!! By- the -way a travel tip;
    I would avoid going anywhere near the whole of Eastern
    Tennessee..(wink!)...rer


 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project