    I've been jonesing for a laser welder lately -- it's nice to see
    someone else is really enthused by its capabilities. Have you tried
    fusing different types of metals together with it? I do a lot of
    copper/silver pieces, and it would be so nice to not have to deal
    with the excessive oxidation that the copper develops so early on,
    making it hard to get solder to flow, etc. I honestly haven't seen
    but one laser welder in person, and it was not available for demo,
    so I didn't get to see it in action. Which one did you get? Would you
    recommend it specifically? I am working on taking out a small
    business loan to try and beef up the studio a little, and this is
    definitely at the top of my list, since I get so many repair
    requests for itty bitty details on antique pieces, and I'm terrified
    to attempt it with the torch. Plus, I love the idea of maintaining
    the original patina! I don't think I could turn away from the torch
    completely, though -- too much of a pyro love for that! 

Jennie
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project